FIELD: anticorrosive compositions. SUBSTANCE: composition is prepared on the basis of low-molecular butadiene rubber - 100 mas. p. The latter is stirred with 40-50 mas. p. sulfur, 5-10 mas. p. altax, 5-10 mas. p. plasticizer - n-tert. -octylphenolformaldehyde resin, 30-40 mas. p. aerosil and applied on the prepared surface by two layers. Vulcanization is carried out in layers at 150 C x 1 hr. Both layers - at 150 C x 3 hr. Coating properties: impact strength is 5 HM, steel adhesion is 13.0-14.9 MPa, mass change in media: in 20% HCl - 3.2-3.8%, in 20% H2SO4 - 3.4-3.9%, in 20% NaOH - 2.2-3.1%. Composition is used for protection of equipment working in strong corrosive media at increased temperatures. EFFECT: enhanced quality and effectiveness of composition. 6 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
RUBBER COMPOUND | 2001 |
|
RU2235740C2 |
POLYMERIC COMPOSITION | 1997 |
|
RU2145969C1 |
RUBBER COMPOUND | 1994 |
|
RU2083608C1 |
MODIFIED UNSATURATED ELASTOMERS' PRODUCTION PROCESS | 2001 |
|
RU2190625C1 |
RUBBER COMPOUND | 2001 |
|
RU2199557C2 |
BITUMEN-POLYMER COMPOSITION PRODUCTION | 2000 |
|
RU2177969C1 |
RUBBER MIXTURE (VARIANTS) | 2002 |
|
RU2235105C2 |
FIRE-RESISTANT RUBBER MIXTURE | 2011 |
|
RU2472821C1 |
ORGANOSILICON COMPOSITION OF COLD HARDENING | 1996 |
|
RU2105778C1 |
0 |
|
SU1781246A1 |
Authors
Dates
1996-08-20—Published
1992-12-07—Filed