FIELD: tubular electrode for gas-shield arc welding. SUBSTANCE: electrode has ferrum containing tube, filled by charge. Charge including alloying elements and ingredients for fluxing oxides contains (mass%) 40-60 of titanium dioxide, 0.3-0.5 of boron oxide and 1.0-5.0 of aluminium powder. Aluminium powder exhibits higher affinity with oxygen that other components of charge. Quantity of aluminium powder is selected in such a way that to provide in seam metal content of titanium equal to 0.02-0.08%, less than 0.002% of boron and less than 0.10% of aluminium. Filling factor of electrode consists 14-17%. That charge may include silicium dioxide (2.0-4.5)mass %, manganese alloying component - (10.0- 15.0)mass %, nickel -(8.0-10.0)mass %. EFFECT: enhanced quality of welded seam with use of such electrode. 11 cl, 2 dwg, 7 tbl
Title | Year | Author | Number |
---|---|---|---|
SELF-PROTECTION GRANULATED FLUX FOR ELECTRIC ARC WELDING AND METHOD OF ITS PRODUCTION | 1992 |
|
RU2086379C1 |
METHOD OF GAS-SHIELDED ARC WELDING OF STEEL RAILS (VERSIONS) | 1998 |
|
RU2136465C1 |
WELDING ELECTRODE WITH LOW MANGANESE FLUX CORE AND GAS-PRODUCING COATING (VERSIONS) | 2013 |
|
RU2622476C2 |
METHOD OF AND DEVICE FOR PIPE AND TUBE WELDING | 1996 |
|
RU2181320C2 |
CHARGE FOR POWDER WIRE | 0 |
|
SU1433709A1 |
MIXTURE FOR PRODUCING POWDER WIRE | 0 |
|
SU1731549A1 |
WELDING SUPPLY SOURCE AND METHOD OF ITS PROVISION WITH CURRENT | 1994 |
|
RU2100158C1 |
COMPOSITE WIRE FOR ARC WELDING AND BUILDING UP | 2011 |
|
RU2478029C2 |
D C INTERRUPTER | 1998 |
|
RU2140704C1 |
WIRE FEEDING APPARATUS | 1997 |
|
RU2125926C1 |
Authors
Dates
1996-09-27—Published
1993-11-15—Filed