FIELD: mining industry. SUBSTANCE: method comprises consecutive multistep crushing and grinding. The last before grinding crushing step is conducted in high-speed centrifugal impact crusher at the speed of impact of ore lumps against shield within the range 70-150 m/sec until lump size 10/12/-0 mm is achieved. Then crushed ore is ground in conventional ball mill until lump size sufficient for flotation is obtained. EFFECT: optimized operation parameters. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
DEVICE FOR PROCESSING OF MAGNETIC GOLD-CONTAINING SCRAP | 1997 |
|
RU2115746C1 |
METHOD OF ORE PRETREATMENT OF OXIDATED AND MIXED COPPER ORES FOR LEACHING | 2007 |
|
RU2350394C2 |
METHOD OF DRY CONCENTRATION OF WOLLASTONITE ORE | 1999 |
|
RU2142348C1 |
METHOD TO PRODUCE CRUSHED ROCK FROM IRON-CONTAINING MATERIAL | 1991 |
|
RU2043164C1 |
METHOD OF DRESSING OF THE BASE GOLD-QUARTZ AND GOLD-SULFIDE-QUARTZ ORES LOCALIZED IN THE BLACK SHALE ROCKS | 2005 |
|
RU2294800C1 |
METHOD OF FLOTATION EXTRACTION OF SULPHIDE CONCENTRATE FROM SULPHIDE -OXIDISED COPPER ORE | 2007 |
|
RU2352401C2 |
METHOD OF ORE GRINDING | 1994 |
|
RU2056947C1 |
COMPLEX FOR PROCESSING GOLD-CONTAINING ORES | 1997 |
|
RU2123891C1 |
METHOD OF PREPARATION OF SLAG-SODA CHARGE CONTAINING VANADIUM FOR OXIDISING ROASTING AND PROCESSING LINE FOR THIS PROCESS | 2007 |
|
RU2365650C1 |
REPROCESSING METHOD OF METALLURGICAL SLAGS AND PROCESS LINE (VERSIONS) FOR ITS IMPLEMENTATION | 2008 |
|
RU2377324C2 |
Authors
Dates
1996-11-20—Published
1993-08-19—Filed