FIELD: manufacture of abrasive tools. SUBSTANCE: flexible abrasive cloth comprises substrate made of dacron is coated with primer layer of adhesive based on butadiene- styrene-nitrile carboxylate copolymers and layer of abrasive-adhesive composition composed of mixture of the same adhesive, water and abrasive powder. The primer layer and the abrasive-adhesive composition layer are applied to the substrate through controllable gap between working tools. The layers are then dried at room temperature for 30-40 minutes and heat-treated at 130-150 C for 20-30 minutes. EFFECT: improved properties of the abrasive-adhesive composition and more efficient preparation process. 4 cl, 3 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURE OF FLEXIBLE ABRASIVE PLATE | 2001 |
|
RU2215645C2 |
COATED ABRASIVE TOOL | 2012 |
|
RU2605721C2 |
BAND WITH ABRASIVE COATING | 1992 |
|
RU2116186C1 |
GRAINED ABRASIVE, ABRASIVE ARTICLE, AND METHOD OF MANUFACTURING GRAINED ABRASIVE | 1991 |
|
RU2092514C1 |
ABRASIVE ARTICLE AND METHOD OF ITS PRODUCTION | 2008 |
|
RU2453418C2 |
ABRASIVE ARTICLES WHICH INCORPORATE FIXING COATING APPLIED BY LAMINATION | 1994 |
|
RU2125510C1 |
ELECTRIC HEATER AND METHOD TO MANUFACTURE HONEYCOMB HEATING ELEMENT FOR IT | 2011 |
|
RU2483493C2 |
METHOD OF PRODUCING ABRASIVE PAPER | 0 |
|
SU1435415A1 |
ABRASIVE ARTICLE | 2006 |
|
RU2402415C2 |
METHOD OF COMPLEX CORROSION PROTECTION OF EXTENDED STEEL PIPE LINES (VERSIONS) | 2005 |
|
RU2296817C2 |
Authors
Dates
1996-11-20—Published
1994-03-01—Filed