FIELD: ferrous metallurgy. SUBSTANCE: when producing balanced steel microalloyed with vanadium and nitrogen in converter by a method involving blowing metal smelt with oxygen, heating metal, prior to be tapped into ladle, to a temperature by 5- 20 C higher than prescribed temperature, introducing deoxidizing agents, alloying additives, and vanadium slag to metal smelt, and blowing metal in ladle with inert gas, into the ladle, simultaneously with introducing slag nitrogen-containing additives begin to be added and their addition stops when metal tap is finished. EFFECT: facilitated nitrogen content control.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF VANADIUM CONTAINING STEEL | 2006 |
|
RU2334797C2 |
METHOD OF DEOXIDIZING AND ALLOYING VANADIUM-CONTAINING STEEL | 1995 |
|
RU2064509C1 |
METHOD OF MAKING STEEL | 2003 |
|
RU2233339C1 |
METHOD OF CONVERSION OF VANADIUM IRON IN CONVERTER | 1998 |
|
RU2136764C1 |
METHOD OF MANUFACTURING VANADIUM-MICROALLOYED STEEL | 1997 |
|
RU2118380C1 |
METHOD OF SMELTING LOW-CARBON VANADIUM-CONTAINING STEEL OF INCREASED STRENGTH AND COLD RESISTANCE | 2000 |
|
RU2186125C2 |
METHOD OF KILLING AND MICROALLOYING STEEL BY VANADIUM | 1992 |
|
RU2040549C1 |
METHOD OF DEOXIDATION, MODIFICATION AND MICROALLOYING OF STEEL WITH VANADIUM-CONTAINING MATERIALS | 1998 |
|
RU2140995C1 |
METHOD FOR PRODUCTION OF STEEL NATURALLY ALLOYED WITH VANADIUM IN CONVERSION OF VANADIUM IRON IN OXYGEN STEEL-MAKING CONVERTERS BY MONOPROCESS WITH SCRAP CONSUMPTION UP TO 30% | 1997 |
|
RU2105072C1 |
METHOD OF DEOXIDIZATION, MODIFICATION, AND VANADIUM-ALLOYING OF STEEL | 1997 |
|
RU2120477C1 |
Authors
Dates
1996-11-20—Published
1996-04-19—Filed