FIELD: production of composite materials. SUBSTANCE: modified epoxy resins are prepared by interaction of epoxy diane resin with butadiene acrylonitrile caoutchouc by heating, the process takes place in the presence of activating agent. Product of condensation of diacetylferrocene with epichlorhydrin is used as mentioned above activating agent, its quantity being 1.25-5.0 % of mass of epoxy resin. Said interaction is carried out at 25-70 C, mass ratio of resin and caoutchouc being (1-4):1 respectively. EFFECT: simplifies the method.
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR ANTICORROSIVE PROTECTION | 1992 |
|
RU2047632C1 |
FROTHING FILM GLUE COMPOSITION | 1991 |
|
RU2034891C1 |
COMPOSITION FOR ABRASIVE TOOLS AND METHOD OF MANUFACTURING THEREOF | 1995 |
|
RU2104857C1 |
GLUING MASTICS FOR GLUING NITROLINOLEUM AND FACING PLATES TO VARIOUS BASES DURING DECORATION AND REPAIR OPERATIONS IN VARIOUS BUILDINGS | 1994 |
|
RU2083625C1 |
ADHESIVE COMPOSITION | 2003 |
|
RU2247136C1 |
COMPOSITION COMPRISING CARBOXYLATED BUTADIENE-NITRILE RUBBER | 1991 |
|
RU2048490C1 |
COMPOUND FOR SEALING RADIO ELECTRONIC DEVICES | 1987 |
|
SU1501506A1 |
EXTINGUISHANT | 1992 |
|
RU2005517C1 |
LOW-FLAMMABILITY STRUCTURAL FILM ADHESIVE | 2022 |
|
RU2803988C1 |
PROCESS OF PRODUCTION OF HEAT-RESISTANT EPOXIDE COMPOUND FOR GLASS-FIBER MATERIALS | 2006 |
|
RU2299897C1 |
Authors
Dates
1997-01-10—Published
1993-07-27—Filed