FIELD: protective coatings, building materials. SUBSTANCE: surface of parts, in particular, of facing tiles is first covered with printing screen with relative area of openings 10-95% and screen pitch 12-64 cm-1 and then with coating composition containing ethylenically unsaturated compounds. The composition is pressed through and dried at 20-80 C for 5-30 sec. A second monomer- and oligomer-containing layer is finally applied, which is polymerized under UV irradiation. EFFECT: durable, resistant to boiling water material produced. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF POLYESTER COATING | 1995 |
|
RU2084484C1 |
METHOD OF PREPARING PROTECTIVE AND ORNAMENTAL COATING ON BUILDING MATERIAL | 1994 |
|
RU2084429C1 |
PROCESS OF PRODUCTION OF HIGH-REFLECTING THREE-LAYER FILM COATS | 1992 |
|
RU2028984C1 |
METHOD OF OBTAINING POLYMERIC COATING ON SURFACE OF BUILDING PRODUCTS | 1992 |
|
RU2046719C1 |
INKJET PRINTING METHODS FOR DECORATIVE SURFACES | 2017 |
|
RU2743731C2 |
METHOD TO FORM DECORATING COVER ON PIECE SURFACE | 1992 |
|
RU2036248C1 |
DECORATED NATURAL LEATHER | 2018 |
|
RU2745321C1 |
PRODUCTION OF DECORATIVE SURFACES | 2017 |
|
RU2742293C2 |
METHOD FOR INKJET PRINTING FOR DECORATIVE LAYERED PANELS | 2019 |
|
RU2755627C1 |
METHOD OF MAKING DECORATIVE COATING | 2012 |
|
RU2515521C2 |
Authors
Dates
1997-02-27—Published
1993-07-28—Filed