FIELD: organic chemistry. SUBSTANCE: amorphous silicon dioxide is treated with boric acid, heat treated at 400-700 C and washed with hot water. EFFECT: higher efficiency. 4 cl, 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING AMORPHOUS SILICON DIOXIDE FROM RICE HUSK | 1994 |
|
RU2061656C1 |
| METHOD OF PREPARING WATER-SOLUBLE SILICATES FROM RICE HUSK ASHES | 1996 |
|
RU2106304C1 |
| METHOD OF PREPARING BORON CARBIDE, INTERCALATED COMPOUND OF GRAPHITE OXIDE WITH DODECAHYDRO-CLOSO-DODECABORATE ACID, AND METHOD OF SYNTHESIS OF THIS COMPOUND | 1998 |
|
RU2123474C1 |
| SORBENT FOR LIQUID MEDIUM TREATMENT | 1997 |
|
RU2117527C1 |
| VEGETABLE AND ANIMAL OILS AND FATS | 2009 |
|
RU2515970C2 |
| METHOD FOR PRODUCTION OF SORBENT FOR SEPARATION OF PROTEINS | 1991 |
|
RU2026732C1 |
| SOLUTION FOR PRELIMINARY PREPARATION OF SURFACE OF PLASTICS FOR APPLYING METAL COATINGS | 1995 |
|
RU2077605C1 |
| METHOD OF PREPARING TRITERPENE GLYCOSIDE 3-0-D-GLUCOPYRANOSYL-((1-2)-L)-ARABINOPYRANOSIDE, HEDERAGENINE | 1994 |
|
RU2064934C1 |
| METHOD FOR ADSORPTION REFINING PLANT OIL | 2008 |
|
RU2392299C2 |
| METHOD FOR REFINING RAW VEGETABLE OILS | 0 |
|
SU1033007A3 |
Authors
Dates
1997-06-10—Published
1994-02-16—Filed