FIELD: production of refractory materials. SUBSTANCE: raw materials mixture comprises, mas.% finely dispersed waste of petrochemical industry, 42.5-59.8; phosphoric acid, 25-50; titanium dioxide, 6-15; boron-containing component (as calculated for boron dioxide), 2.2-5. Waste of petrochemical industry comprises aluminium oxide Al2O3 and chromium oxide Cr2O3, their quantities are 85-87 and 13-15 mas.%, respectively. Calcium borate or boric acid are used as said boron-containing component. EFFECT: improved quality. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY MASONRY MORTAR | 1995 |
|
RU2101256C1 |
REFRACTORY LAYING MATERIAL | 1995 |
|
RU2100319C1 |
RAW MIX FOR PREPARING PHOSPHATE BINDER | 1997 |
|
RU2129104C1 |
REFRACTORY MASS | 2001 |
|
RU2212387C2 |
REFRACTORY MASS | 1992 |
|
RU2085533C1 |
RAW MATERIALS MIXTURE FOR PRODUCTION OF PHOSPHATE BINDER | 1996 |
|
RU2111185C1 |
RAW MEAL FOR MANUFACTURING REFRACTORY MATERIALS | 2001 |
|
RU2213715C2 |
PHOSPHATE BINDER FOR PREPARING REFRACTORY COMPOSITIONS | 1997 |
|
RU2139836C1 |
REFRACTORY MASS | 1993 |
|
RU2081863C1 |
PHOSPHATE BINDER FOR PRODUCTION OF HIGH-MELTING COMPOSITIONS | 2004 |
|
RU2279413C2 |
Authors
Dates
1997-06-10—Published
1994-05-25—Filed