FIELD: sorption technique. SUBSTANCE: method involves impregnation of coal particles with solution of catalytic additives and with 0.2-0.8 mass % solution of triethylene diamine. Said impregnation is carried out at volume ratio of coal and impregnating solution 1:0.2-0.4. The process is followed by heat treatment at 110-150 C. EFFECT: increased dynamic activity of sorbent-catalyst.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING SORBENT-CATALYST | 1995 |
|
RU2083274C1 |
METHOD OF PREPARING SORBENT-CATALYST | 1997 |
|
RU2108149C1 |
SORBENT-CATALYST PREPARATION METHOD | 2002 |
|
RU2202410C1 |
SORBENT-CATALYST PREPARATION METHOD | 2003 |
|
RU2236902C1 |
METHOD OF PRODUCTION OF SORBENT-CATALYST | 2005 |
|
RU2281158C1 |
CATALYST PREPARATION PROCESS | 2003 |
|
RU2228902C1 |
METHOD FOR PRODUCTION OF SORBENT CATALYST | 2003 |
|
RU2247598C1 |
METHOD OF PRODUCTION OF SORBENT-CATALYST | 2004 |
|
RU2254915C1 |
METHOD FOR OBTAINING A CATALYST | 2022 |
|
RU2800454C1 |
METHOD OF REGENERATION OF SORBENTS-CATALYSTS FROM INACTIVATED PROTECTIVE MEANS | 2005 |
|
RU2287364C2 |
Authors
Dates
1997-06-20—Published
1994-09-09—Filed