FIELD: television screens. SUBSTANCE: reactor is filled with demineralized water, to which europium-activated luminophor based on yttrium oxide and/or oxysulfide is added under stirring. Into the second reactor with water, iron oxide suspension containing 0.01-1 g oxalic acid per 1 kg luminophor is added. Pigment suspension is added to luminophor suspension under stirring. Precipitate is filtered off and dried at 110 C. EFFECT: satisfactory quality of pigment-to-luminophor adhesion and density of crystal package in mosaic elements with high light parameters of kinescope retained.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SURFACE TREATMENT OF LUMINOPHORS | 1993 |
|
RU2082743C1 |
METHOD OF OBTAINING PIGMENTED RED HEAT LUMINOPHORE BASED ON YTTRIUM OXISULFIDE | 0 |
|
SU1773927A1 |
POLYMERIC COMPOSITION FOR MAKING FILM FOR GREEN HOUSES | 1996 |
|
RU2125069C1 |
METHOD OF PREPARING OF PIGMENTED LUMINOPHORE ON YTTRIUM OXYSULFIDE-BASE WITH RED COLOR LUMINESCENCE | 0 |
|
SU1819906A1 |
METHOD OF PRODUCTION OF CERAMIC ZIRCONIUM PIGMENTS | 1997 |
|
RU2117018C1 |
METHOD FOR PRODUCTION OF RED IRON-OXIDE PIGMENT WITH PRESET ELECTROKINETIC CHARACTERISTICS | 1991 |
|
RU2035479C1 |
METHOD OF DETERMINING IMPURITIES IN SCANDIUM OXIDE | 1994 |
|
RU2091791C1 |
METHOD OF LUMINESCENT DETERMINATION OF EUROPIUM ADMIXTURES | 0 |
|
SU1332202A1 |
APPARATUS FOR GROWING OF SPIRULINE PLATENSIS MICROALGAE | 1999 |
|
RU2163069C2 |
METHOD FOR PRODUCTION OF HEAT-RESISTANT CERAMIC PIGMENTS | 1991 |
|
RU2044013C1 |
Authors
Dates
1997-06-27—Published
1993-07-01—Filed