FIELD: metallurgy; applicable in processing of metal-containing slime wastes. SUBSTANCE: the offered method includes mixing of wet slime with dry powdery sodium silicate in the amount of 3-10% of slime mass, molding of obtained mixture, for instance, by means of press or by extruder, drying at temperature of 300-350 C and melting of briquetted product in induction furnaces. EFFECT: higher efficiency.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING METAL-CONTAINING SLUDGES | 1994 |
|
RU2097166C1 |
METHOD FOR PROCESSING OF INDUSTRIAL WATER-AND-OIL CONTAINING WASTES | 2000 |
|
RU2213153C2 |
METHOD FOR PROCESSING METAL-CONTAINING SLIMES | 2002 |
|
RU2237544C2 |
METHOD OF PROCESSING METALLIFERROUS WASTE AND DEVICE FOR PROCESSING THE WASTE | 2001 |
|
RU2217510C2 |
COMPLEX WASTELESS TREATMENT OF TOXIC WASTES | 2009 |
|
RU2484868C2 |
METHOD OF BRIQUETTING METAL CHIPS | 2003 |
|
RU2266968C2 |
PROCEDURE FOR PURIFYING RETURN WATER OF GAS CLEANING IN SMELTING FURNACES, UTILISATION OF METAL CONTAINING SLIMES AND DEVICE FOR IMPLEMENTATION OF THIS PROCEDURE | 2009 |
|
RU2413015C2 |
IRON-CONTAINING MATERIAL PROCESSING METHOD | 2011 |
|
RU2466196C1 |
METHOD FOR OBTAINING BRIQUETTE TO OBTAIN TITANIUM- AND ZIRCONIUM-CONTAINING CAST IRON | 2012 |
|
RU2510684C1 |
METHOD OF PRODUCING TECHNICAL SILICON | 2019 |
|
RU2703084C1 |
Authors
Dates
1997-07-10—Published
1994-01-10—Filed