FIELD: chemical industry. SUBSTANCE: prior to deactivation of catalyst, polymerizate is kept for 2 to 7 hours at α-catalyst to promoter weight ratio of (1.5:12.0):1. EFFECT: reduced toxicity and smell of synthetic film-forming substances, higher softening temperature, greater elasticity and stronger adhesion of coating to metal.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF SYNTHETIC DRYING OIL | 1995 |
|
RU2086568C1 |
METHOD OF SYNTHETIC FILM-FORMING MATERIAL PRODUCING | 1994 |
|
RU2068854C1 |
METHOD OF SYNTHESIS OF SYNTHETIC FILM-FORMING AGENT | 1994 |
|
RU2081885C1 |
METHOD OF SYNTHETIC DRYING OIL PRODUCING | 1995 |
|
RU2116320C1 |
METHOD OF PREPARING FILM-FORMING PETROLEUM POLYMERIC RESIN | 1993 |
|
RU2117013C1 |
METHOD OF PREPARING SYNTHETIC FILM FORMING AGENT | 1999 |
|
RU2150477C1 |
METHOD OF PREPARING SYNTHETIC FILM-FORMING MATERIAL | 2000 |
|
RU2194723C2 |
PROCESS FOR PRODUCING SYNTHETIC PAINTING OIL | 0 |
|
SU1027174A1 |
METHOD OF PREPARING PIPERYLENE OLIGOMERS | 1997 |
|
RU2135442C1 |
COMPOSITION FOR COATINGS | 1995 |
|
RU2089581C1 |
Authors
Dates
1997-07-20—Published
1994-10-11—Filed