FIELD: petrochemical and paint-and-varnish industry. SUBSTANCE: cooligomerization of components of piperylene-containing mixes is carried out at 50-120 C. Catalyst is titanium tetrachloride, promoter is mixture of lower carbonyl compound with water. After cooligomerization, polymerizate is maintained at 50-120 C, light C5-C7 hydrocarbons are degassed, and the resulting product is maintained at 50-120 C for 10-25 h, catalyst is then deactivated and light hydrocarbons are degassed. Catalyst promoter is introduced into polymerizate at each maintenance stage. EFFECT: lower amount of siccative used stabilized whiteness of white paint and higher water resistance. 1 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING SYNTHETIC FILM-FORMING MATERIAL | 2000 |
|
RU2194723C2 |
METHOD FOR PRODUCTION OF SYNTHETIC DRYING OIL | 1995 |
|
RU2086568C1 |
METHOD OF PREPARING PIPERYLENE OLIGOMERS | 1997 |
|
RU2135442C1 |
METHOD OF SYNTHESIS OF SYNTHETIC FILM-FORMING AGENT | 1994 |
|
RU2081885C1 |
METHOD OF SYNTHETIC DRYING OIL PRODUCING | 1995 |
|
RU2116320C1 |
PROCESS FOR PREPARING SYNTHETIC FILM-FORMING SUBSTANCE | 1994 |
|
RU2084464C1 |
METHOD OF PREPARING FILM-FORMING PETROLEUM POLYMERIC RESIN | 1993 |
|
RU2117013C1 |
COMPOSITION FOR COATINGS | 1999 |
|
RU2161634C2 |
METHOD OF FILM-FORMING AGENT | 1999 |
|
RU2161629C2 |
METHOD OF SYNTHETIC FILM-FORMING MATERIAL PRODUCING | 1994 |
|
RU2068854C1 |
Authors
Dates
2000-06-10—Published
1999-03-01—Filed