FIELD: autonomous power supplies which use solar power. SUBSTANCE: method involves application of ethylene co-polymer films with vinyl acetate and external coating on front and back sides of photodetector. Before deposition coating is treated by beam of accelerated electrons of 0.5-1.5 MeV power until gel fraction content of 10-50 % is reached. Then assembled unit is sealed and processed at temperature of at least 130 C for at least 3 min. EFFECT: increased functional capabilities.
Title | Year | Author | Number |
---|---|---|---|
PHOTOELECTRIC MODULE | 1992 |
|
RU2069920C1 |
PHOTOELECTRIC MODULE AND PROCESS OF ITS MANUFACTURE | 2002 |
|
RU2214020C1 |
MULTILAYER LAMINATED GLASS | 1993 |
|
RU2036870C1 |
PHOTOELECTRIC MODULE | 2005 |
|
RU2287207C1 |
METHOD OF MANUFACTURING OPTICALLY TRANSPARENT ADHESIVE FILM | 1993 |
|
RU2084342C1 |
PHOTOELECTRIC UNIT | 1993 |
|
RU2086046C1 |
PHOTOELECTRIC MODULE | 1991 |
|
RU2008749C1 |
PROTECTIVE COAT FOR PHOTOELECTRIC MODULE | 2002 |
|
RU2214019C1 |
FLEXIBLE MODULE OF SOLAR BATTERY | 2003 |
|
RU2234166C1 |
METHOD OF MANUFACTURING POLYMER PRODUCT, POLYMER COMPOSITION FOR MANUFACTURE THEREOF, AND MODIFIER CONTAINED IN THIS COMPOSITION | 2002 |
|
RU2203913C1 |
Authors
Dates
1997-07-27—Published
1995-04-12—Filed