FIELD: welding materials for high and medium- carbon steels. SUBSTANCE: coating contains (in wt %): electrode coating blend, 53-60; wood meal, 5-7; baddeleyte concentrate , the balance. Electrode coating is, in turn, composed of (in wt %): rutile, 48; feldspar, 30; ferro-manganese, 15; magnesite, 5; and dextrin, 2. Chief components of baddeleyte are (in wt %): zirconium oxide, 47-49; silicon oxide, 20.2-21.5; calcium oxide, 4.02-4.8; iron oxides, 1.5-2.2; and aluminium oxide, 1.3-1.5. EFFECT: increased reliability of welding seam, improved stability of arc burning, and avoided heat treatment of welding join. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTRODE COAT | 1995 |
|
RU2107602C1 |
ELECTRODE COATING CHARGE | 2001 |
|
RU2196034C2 |
METHOD TO PRODUCE COMPOSITION MATERIAL BASED ON TUNGSTEN-COPPER PSEUDOALLOY | 1993 |
|
RU2043867C1 |
METHOD FOR PRODUCTION OF CERAMIC MATERIAL BASED ON ZIRCONIUM DIBORIDE | 1992 |
|
RU2053209C1 |
ELECTRODE COATING CHARGE | 2001 |
|
RU2196033C2 |
METHOD OF PREPARING COMPOSITE POWDERY MATERIAL OF ZIRCONIUM-CONTAINING MINERAL STOCK | 1999 |
|
RU2167128C2 |
METHOD OF MANUFACTURING COMPOSITE MATERIAL FROM TUNGSTEN-CONTAINING MINERAL RAW MATERIAL | 1995 |
|
RU2098232C1 |
ELECTRODE FLUX | 2012 |
|
RU2504465C1 |
METHOD FOR PRODUCING ELECTRODES OF TUNGSTEN BEARING MINERALS AND DEVICE TO IMPLEMENT THE SAME | 1993 |
|
RU2043862C1 |
WELDING ELECTRODE | 0 |
|
SU1738567A1 |
Authors
Dates
1997-08-20—Published
1995-03-03—Filed