FIELD: technology of preparation of synthetic wollastonite. SUBSTANCE: claimed method of preparing electrothermal phosphorus slag based wollastonite comprises adding additives to slag in reducing atmosphere, sharply cooling the melt and thermally treating it. The additives include sodium and barium sulfates, vanadium oxide and calcium fluoride, and the are added to attain molar ratio of in the melt. Thermal treatment is carried out in two stages at 720-740 C for 30 minutes and at 950-1010 for 2.5 hours. Vanadium quartzite containing CaF2,BaSO4,V2O5 may be used as the final product. EFFECT: lower heat treatment temperature. 3 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RECOVERY OF VANADIUM FROM TITANIUM-VANADIUM SLAG | 2008 |
|
RU2365649C1 |
METHOD OF AMMONIA OXIDATION USING OXIDE CATALYST OF CELLULAR STRUCTURE AND METHOD OF CATALYST PREPARATION | 1997 |
|
RU2127223C1 |
PROCEDURE FOR BLAST MELTING TITANIUM-MAGNETITE RAW MATERIAL | 2008 |
|
RU2385352C2 |
METHOD FOR MANUFACTURING OF PORTLAND CEMENT AND FERROCONCRETE ARTICLES ON THE BASE OF PORTLAND CEMENT | 1995 |
|
RU2060978C1 |
COLOURED SLAG-STONE CAST PRODUCT AND MIXTURE FOR MAKING SAID PRODUCT | 2011 |
|
RU2474541C1 |
PROCEDURE FOR PROCESSING VANADIUM CONTAINING IRON | 2008 |
|
RU2385349C2 |
METHOD OF PREPARING VANADIUM COMPOUNDS | 1998 |
|
RU2124479C1 |
HEAT-INSULATING MIXTURE FOR CONTINUOUS CASTING OF STEEL | 1999 |
|
RU2175279C2 |
WELDING FLUX | 2001 |
|
RU2207237C2 |
PORTLAND CEMENT PRODUCTION METHOD AND PORTLAND CEMENT BASED CONCRETE AND REINFORCED CONCRETE PIECES PRODUCTION METHOD | 1995 |
|
RU2060979C1 |
Authors
Dates
1997-09-10—Published
1994-07-13—Filed