FIELD: chemical industry. SUBSTANCE: product from reactive SiO2, Al2O3 and P2O5 and matrix organic material is prepared by mixing Al2O3 with P2O5 and hydrochloric acid followed by addition of SiO2 and matrix material to the mixture and crystallization of the product on heating the resulting gel. Al2O3 and SiO2 are used in the same molar ratios as in the desired product, and P2O5 is added in excess of stoichiometric amount. SiO2 to hydrochloric acid ratio is 0.3-3.0. The desired product has improved resistance to deactivation by coking. EFFECT: more efficient preparation method. 8 cl, 7 tbl
Authors
Dates
1997-09-27—Published
1992-12-09—Filed