FIELD: metallurgical industry. SUBSTANCE: refractory comprises, wt.-%: tricalcium silicate, 47.1-77; dicalcium silicate, 10-24.9; periclase, 10-20; and calcium alumoferrites, 3-8. Characteristics: slag wear resistance is 12-15 %; thermal resistance (1300 C water) is 4 or 5 heat cycles; ultimate compression strength 57-70 G/sq.mm; initial softening temperature under load conditions is 0.2 H/sq.mm is 1530-1620 C. Maximum application temperature is 1600-1700 C. EFFECT: improved properties. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
UNROASTED LIME-SILICATE-PERICLASE REFRACTORY | 1996 |
|
RU2094408C1 |
LIMESTONE-SILICATE-PERICLASE CLINKER | 1996 |
|
RU2094406C1 |
ROASTINGLESS REFRACTORY MATERIAL | 1982 |
|
RU2016875C1 |
MAGNESIA-SPINELLIDE REFRACTORY MATERIAL | 2002 |
|
RU2198859C1 |
PERICLASE-SPINEL REFRACTORY | 1998 |
|
RU2124487C1 |
PERICLASE-SPINEL REFRACTORY | 2015 |
|
RU2623760C2 |
PERICLASE CLINKER | 1996 |
|
RU2085537C1 |
SPINEL-PERICLASE-CARBON REFRACTORY MATERIAL | 1996 |
|
RU2068823C1 |
PERICLASS-SPINELLIDE REFRACTORY | 1999 |
|
RU2142926C1 |
ROASTING-FREE REFRACTORY MATERIAL | 1999 |
|
RU2150441C1 |
Authors
Dates
1997-10-27—Published
1996-01-19—Filed