FIELD: machining; applicable in machining with preliminary heating, particular, wheel pairs of rolling stock. SUBSTANCE: to prevent cold working and defects of disturbed roll surface continuity, machining is carried out with plasma heating of treated surface with direct plasma arc, for which purpose, it is located before cutter at distance of 100-200 mm with spaced relation of 25-30 mm between plasma generator and roll surface; and depth of cutting, and arc current intensity are taken 2 mm and 180 A depending on depth of detected defects on roll surface. EFFECT: higher efficiency. 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR RECOVERING PROFILE OF ROLLING SURFACE OF WHEELS OF RAIL VEHICLES | 2020 |
|
RU2754627C1 |
METHOD FOR RESTORING THREAD SURFACE PROFILE OF RAIL TRANSPORT WHEELS | 2022 |
|
RU2809615C1 |
REST OF WHEEL TURNING LATHE | 2001 |
|
RU2208501C2 |
METHOD OF FABRICATING WORK HOLDERS OF TUBE MILLS AT LENGTHWISE TUBE ROLLING | 2006 |
|
RU2327749C1 |
CUTTING PLATE USED IN LATHE FOR TURNING RIM OF RAILWAY ROAD WHEEL AND METHOD FOR MAKING SUCH PLATE | 2001 |
|
RU2196026C2 |
TANGENTIAL CUTTING TIP | 2001 |
|
RU2201317C2 |
CARRIAGE OF WHEEL LATHE AND FORMING TOOL TO MACHINE WHEEL PAIRS | 1999 |
|
RU2152848C1 |
CUTTING TIP | 2000 |
|
RU2198767C2 |
SAFETY AND VENTILATION ARRANGEMENT FOR LATHE FOR PLASMA-MECHANICAL WORKING | 0 |
|
SU1268373A1 |
WHEELSET TIRE PROFILE PROCESSING DEVICE WITHOUT ROLL-OUT | 2019 |
|
RU2717756C1 |
Authors
Dates
1997-11-20—Published
1996-02-19—Filed