FIELD: production of ferroalloys, particular, smelting of ferrosilicon in blast furnace. SUBSTANCE: the offered charge includes coke, flux, iron ore materials and shungite with ratio C:SiO O2 = 0.25-0.6 in the amount of 16-50%. EFFECT: higher efficiency of smelting of ferrosilicon. 1 tbl