FIELD: catalysts for petrochemical syntheses. SUBSTANCE: as iron oxide-based catalyst, exhausted catalyst is used after treatment with water in weight ratio 1:(0.12-0.20) at 20-30 C for 5-10 h followed by adding missing promoting additives and finally agitating mixture in presence of 1.6 to 2 weight parts of carbon dioxide per 1 part of catalyst. EFFECT: completely reused exhausted catalyst and avoided formation of waste water and loss of promoter. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD TO PRODUCE CATALYST FOR DEHYDROGENATION OF ALKYLBENZENES | 1994 |
|
RU2064829C1 |
CATALYST FOR OXIDIZING ORGANIC COMPOUNDS | 1993 |
|
RU2047352C1 |
METHOD OF CATALYTIC PURIFICATION OF GAS RELEASES FROM SYNTHETIC RUBBER PRODUCTION IN PRESENCE OF OZONE | 1995 |
|
RU2085265C1 |
METHOD OF STABILIZATION OF EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130031C1 |
METHOD OF PREPARING THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2113445C1 |
METHOD FOR PRODUCTION OF BUTADIENE-STYRENE(α-METHYL STYRENE) RUBBER BEING MODIFIED BY POLAR MONOMER | 1996 |
|
RU2115664C1 |
GLUE MELT | 1993 |
|
RU2110548C1 |
MOLTEN ADHESIVE | 1994 |
|
RU2100397C1 |
METHOD OF PREPARING POLYMERIC AMINE ANTIOXIDANT | 1996 |
|
RU2130033C1 |
BITUMEN COMPOSITION | 1995 |
|
RU2093538C1 |