FIELD: carbon materials. SUBSTANCE: graphite powder is mixed with thermoplastic binding agent and mixture is placed into metal cartridge of press mold matrix, heated to binder melting temperature, polymerized, and cooled to ambient temperature in press mold at constant pressure. EFFECT: improved quality of press molds and simplified their manufacture. 4 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING THE DIAMOND TOOL | 1993 |
|
RU2049655C1 |
MATERIAL FOR DIES OF DIAMOND AND ABRASIVE TOOLS AND METHOD OF MANUFACTURING THEREOF | 1998 |
|
RU2136479C1 |
METHOD OF MANUFACTURE OF DIAMOND ROCK-CUTTING TOOL | 1998 |
|
RU2156186C2 |
METHOD FOR MANUFACTURE OF TOOLS | 1993 |
|
RU2071913C1 |
DIAMOND DRILL BIT | 1996 |
|
RU2112131C1 |
DIAMOND DRILL BIT WITH AIR BLOW-THROUGH | 1999 |
|
RU2167260C1 |
ABRASIVE CUTTING TOOL | 1993 |
|
RU2083352C1 |
METHOD OF DIAMOND TOOL MANUFACTURE | 1999 |
|
RU2175590C2 |
DIAMOND TOOL FOR ROCK BREAKING | 2001 |
|
RU2202444C2 |
DIAMOND DRILLING BIT MANUFACTURING METHOD | 2006 |
|
RU2314908C2 |
Authors
Dates
1998-07-27—Published
1996-01-24—Filed