FIELD: ferrous metallurgy, namely production of commercial vanadium cast iron and production of conversion cast iron. SUBSTANCE: cast comprising carbon, silicium, manganese, vanadium, titanium, copper, nickel, cobalt, chromium, aluminium, germanium and ferrum additionally comprises phosphorous, sulfur and scandium. Content of these components, mas.% is as follows: carbon, 3.0-4.8; silicium, 0.02-0.8; manganese, 0.01-1.5; vanadium, 0.03-1.0; titanium, 0.02-0.8; phosphorous, 0.015-0.10; sulfur, 0.010-0.05; copper, 0.01-0.12; nickel, 0.02-0.3; cobalt, 0.01-0.14; chromium, 0.02-0.9; aluminium, 0.01-0.15; germanium 0.0001-0.002; scandium, 0.0001-0.015; ferrum, the balance. When desired cast iron is used as conversion one then fuel expense and expense for iron-ore portion of charge are decreased by 5-10 %, degree of conversion of vanadium into slag is increased by 0.9-1.5 %, degree of extraction of chromium and vanadium is increased by 1.3-2.2 %; wear resistance of construction steel and cast iron is increased. EFFECT: improved quality of desired product. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
CAST IRON | 1994 |
|
RU2116372C1 |
CONVERSION CAST IRON | 1986 |
|
SU1389315A1 |
METHOD AND CHARGE FOR MANUFACTURE OF STRUCTURAL CARBON STEEL WITH REDUCED HARDENING CAPACITY IN STEEL-MAKING ARC-TYPE FURNACE | 2012 |
|
RU2534715C2 |
CAST IRON | 1999 |
|
RU2148103C1 |
COMPLEX FLUX FOR REMOVAL OF VANADIUM FROM CAST IRON | 1998 |
|
RU2148654C1 |
FUSING AGENT FOR DEVANADIUMIZATION OF CAST IRON | 1986 |
|
RU1412316C |
METHOD AND CHARGE FOR MANUFACTURING OF STRUCTURAL STEEL WITH REDUCED HARDENABILITY | 2007 |
|
RU2363736C2 |
METHOD OF REFINING VANADIUM CAST IRONS IN STEELMAKING UNITS | 1997 |
|
RU2122587C1 |
EXTRA THIN-WALL TUBE FROM AUSTENITE BORON-CONTAINING STEEL FOR COVER OF FUEL ELEMENT, AND METHOD FOR ITS MANUFACTURE | 2009 |
|
RU2420600C1 |
AUSTENITE STEEL | 2003 |
|
RU2233906C1 |
Authors
Dates
1998-07-27—Published
1994-09-05—Filed