METHOD OF PREVENTION OF CORROSION CRACKING UNDER STRESS OF PIPE LINES Russian patent published in 1998 - IPC

Abstract RU 2120079 C1

FIELD: construction; erection and operation of pipe lines. SUBSTANCE: in manufacture of welded straight-seamed pipes, revealed zones of concentration of stresses are marked to introduce correction factors for rated resistance. In welding the pipe line, marked zones are located beyond level of underground water; to this end, pipe line is laid 0.2 m higher or 0.2 m lower relative to underground water level from lower or upper generatrix of pipe line, respectively. Level of underground water is regulated on operating pipe line by means of supporting walls, drainage canals or by deepening the pipe line. EFFECT: enhanced reliability. 2 cl, 3 dwg, 1 tbl

Similar patents RU2120079C1

Title Year Author Number
METHOD FOR PREVENTING STRESS CORROSION CRACKING IN UNDERGROUND PIPELINES 2017
  • Aginej Ruslan Viktorovich
  • Guskov Sergej Sergeevich
  • Musonov Valerij Viktorovich
  • Spiridovich Evgenij Appolinarevich
RU2638121C1
METHOD OF PREVENTION OF CRACKING CORROSION OF PIPE LINE UNDER ACTION OF STRESSES (VERSIONS) 2003
  • Korolev M.I.
  • Volgina N.I.
  • Saljukov V.V.
  • Kolotovskij A.N.
  • Voronin V.N.
RU2247892C2
METHOD OF PREVENTION OF BREAK OF GAS LINES 1998
  • Lisin V.N.
  • Budzuljak B.V.
  • Puzhajlo A.F.
  • Spiridovich E.A.
  • Lisin I.V.
  • Shchegolev I.L.
RU2138725C1
METHOD OF REVEALING SECTION OF MAIN PIPE LINES PREDISPOSED TO CORROSION CRACKING UNDER STRESS (STRESS CORROSION) 1999
  • Lisin V.N.
  • Puzhajlo A.F.
  • Spiridovich E.A.
  • Shchegolev I.L.
  • Lisin I.V.
  • Shajkhutdinov A.Z.
RU2147098C1
METHOD OF DETECTION OF GAS LINES SUBJECTED TO CORROSION CRACKING UNDER STRESS 2001
  • Asadullin M.Z.
  • Askarov R.M.
  • Aminev F.M.
  • Usmanov R.R.
  • Ismagilov I.G.
  • Khakhalkin G.I.
  • Fajzullin S.M.
RU2216681C2
SECTIONAL PIPE FOR ERECTION OF PIPE LINES AND METHOD OF MANUFACTURE OF SUCH PIPE 2003
  • Baranov Vladimir Nikitich
  • Vinogradov Jurij Vasil'Evich
  • Bednjakov Vladimir Vladimirovich
  • Khomenko Vladimir Ivanovich
  • Papkov Oleg Sergeevich
  • Baranov Boris Stepanovich
  • Akhmedshin Rauf Islamovich
  • Novitskij Aleksandr Fedorovich
RU2282091C2
METHOD OF CHECKING PIPELINE PREDISPOSED TO CORROSION CRACKING UNDER LOADS 2004
  • Korolev Mikhail Ivanovich
  • Ilatovskij Jurij Vital'Evich
  • Kharionovskij Vladimir Vasil'Evich
  • Volgina Natal'Ja Ivanovna
  • Saljukov Vjacheslav Vasil'Evich
  • Kolotovskij Aleksandr Nikolaevich
  • Voronin Valerij Nikolaevich
RU2332609C2
EVALUATION METHOD OF STRESS CORROSION CRACKING RESISTANCE OF LOW-ALLOYED PIPE STEELS 2015
RU2611699C1
METHOD OF DETECTING PIPE SECTIONS, PRONE TO INTERNAL CORROSION 2008
  • Petrov Nikolaj Georgievich
  • Popenko Aleksandr Nikolaevich
  • Prokhozhaev Oleg Timofeevich
  • Kochubej Aleksej Dmitrievich
  • Rjabich Nadezhda Konstantinovna
RU2360230C1
METHOD FOR FLAW DETECTION OF MAIN PIPE-LINES IN SECTIONS PREDISPOSED TO CORROSION CRACKING UNDER VOLTAGE 2003
  • Korolev M.I.
  • Volgina N.I.
  • Saljukov V.V.
  • Kolotovskij A.N.
  • Voronin V.N.
  • Urusov V.S.
RU2245540C2

RU 2 120 079 C1

Authors

Lisin V.N.

Spiridovich E.A.

Puzhajlo A.F.

Jakovlev A.Ja.

Markelov V.A.

Kenegesov Ju.T.

Lisin I.V.

Dates

1998-10-10Published

1997-12-26Filed