FIELD: furniture and building industries, and finishing work. SUBSTANCE: composition comprises sawdust and polyethylene according to 1-st embodiment and further comprises solution of natural bischofite, the ratio of components is as follows, wt.pts: sawdust, 100; polyethylene, 30-100; bischofite solution, 10-20 and according to 2nd embodiment, the composition comprises sawdust and polyethylene and further comprises solution of natural bischofite and industrial asbestos production waste in the form of asbestos dust, the ratio of components is as follows, wt.pts: saw dust, 100; polyethylene, 90-100; solution of bischofite, 10-30; asbestos dust, 5-20. EFFECT: reduced combustibility of wood and polymeric materials. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
WOOD-POLYMER COMPOSITES OF LOW FLAMMABILITY AND METHOD OF THEIR PRODUCTION | 2018 |
|
RU2731268C2 |
COMPOSITION FOR MANUFACTURING WOOD CHIPBOARDS | 2002 |
|
RU2206585C1 |
WOOD-POLYMER COMPOSITION | 2020 |
|
RU2753628C1 |
WOOD AND POLYMER COMPOSITION | 2011 |
|
RU2484110C2 |
POLYMER COMPOSITION | 2002 |
|
RU2221824C1 |
CHLOROSULFONATED-BASE POLYETHYLENE COMPOSITION AND METHOD OF PREPARING COATINGS BASED THEREON | 1999 |
|
RU2171269C2 |
HEAT-INSULATING MATERIAL AND METHOD OF ITS PRODUCTION | 2012 |
|
RU2501761C1 |
COMPOSITION FOR FIBROUS MATERIAL AND METHOD OF ITS PRODUCTION | 2011 |
|
RU2478546C1 |
ENVIRONMENTALLY APPROPRIATE WOOD-FILLED PLASTIC AND METHOD OF PREPARATION THEREOF | 1995 |
|
RU2081135C1 |
RIGID POLYVINYL CHLORIDE-BASED WOOD-POLYMER COMPOSITION | 2010 |
|
RU2450037C1 |
Authors
Dates
1999-01-20—Published
1997-01-22—Filed