FIELD: mechanical engineering and other branches of industry. SUBSTANCE: first part of friction pair is oxidized by building up of oxide primarily inside part till relation of its internal and external layers equals 2-4 at electrolyte temperature of 35-45 C, with holding time of up to 40 min and current density of 8-12 A/sq.dm. Second part of friction pair is oxidized by building up to oxide primarily outside the part till relation of its internal and external layers equals 0.25-0.5 at electrolyte temperature not exceeding 5 C, with holding time of up to 30 min and current density of 8-12 A/sq.dm. EFFECT: enhanced wear resistance. 7 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ELECTROCHEMICAL OXIDATION OF COATINGS ON VALVE METALS OR ALLOYS | 2019 |
|
RU2718820C1 |
METHOD OF OBTAINING COMPATIBILITY OF FRICTION PAIRS FOR INTERNAL COMBUSTION ENGINES | 1996 |
|
RU2119587C1 |
METHOD OF COATING DEPOSITION | 1998 |
|
RU2136788C1 |
PROCESS OF BLAST PRESSING OF ARTICLES FROM POWDER MATERIALS | 1997 |
|
RU2128101C1 |
PROCESS OF MICROPLASMA OXIDATION OF VALVE METALS AND THEIR ALLOYS AND GEAR FOR ITS IMPLEMENTATION | 1997 |
|
RU2124588C1 |
INTERNAL COMBUSTION ENGINE WITH PARTS PROVIDED WITH SURFACE COATING AND INSTALLATION FOR MAKING SUCH COATING | 1998 |
|
RU2143573C1 |
METHOD OF PRODUCING ELECTROCHEMICAL OXID-ANODE DIAMOND-CONTAINING COATING OF ALUMINIUM AND ITS ALLOYS | 2016 |
|
RU2631374C2 |
METHOD OF COATINGS APPLICATION | 2000 |
|
RU2166570C1 |
METHOD OF PRODUCTION OF OXIDE COMPOSITE COAT ON ALUMINIUM AND ITS ALLOYS | 2000 |
|
RU2169800C1 |
PROCESS FOR PRODUCING LAMINATED ARTICLES FROM COMPOSITE POLYMERIC MATERIALS | 0 |
|
SU1643162A1 |
Authors
Dates
1999-09-20—Published
1998-02-24—Filed