FIELD: treatment of article surface; applicable in mechanical engineering and instrumentation engineering. SUBSTANCE: method includes article oxidation for 45-100 min with current density of 25-35 A/sq.dm in electrolyte based on boric acid and potassium hydroxide; removal of external layer of coating 10-20 mcm thick and heating of articles with coating at least 70 mcm thick to temperature not below 490 C. Time of holding of article during heating amounts from 50 to 100% of oxidation time. EFFECT: production of articles with increased surface hardness and wear resistance. 1 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF COATING DEPOSITION | 1998 |
|
RU2136788C1 |
METHOD OF OBTAINING CERAMIC COATINGS ON DETAILS FROM STEELS | 2016 |
|
RU2622073C1 |
PROCEDURE FOR APPLYING COATING | 2009 |
|
RU2393274C1 |
METHOD OF MAKING HEAT-RESISTANT INSULATING COATS ON ARTICLES MADE FROM ALUMINUM ALLOYS | 2003 |
|
RU2237758C1 |
METHOD OF COATING OBTAINMENT | 2009 |
|
RU2392359C1 |
METHOD FOR OBTAINING COMPOSITE COATINGS ON VALVE METALS AND THEIR ALLOYS | 2022 |
|
RU2787330C1 |
PRODUCTION OF COATINGS | 2013 |
|
RU2527107C1 |
PROCEDURE FOR APPLICATION OF COATING | 2009 |
|
RU2395633C1 |
METHOD FOR COATING RECEIVING | 2006 |
|
RU2339745C2 |
METHOD OF COATING OBTAINMENT | 2007 |
|
RU2354758C2 |
Authors
Dates
2001-05-10—Published
2000-01-10—Filed