FIELD: chemistry.
SUBSTANCE: method involves electrochemical oxidation in a sulphate electrolyte containing detonation nanodiamonds, using detonation nanodiamonds modified with ammonia, antimony or boron in the amount of 0.5-10.0 g/l.
EFFECT: increasing the microhardness and corrosion resistance of coating, reducing its porosity at low flow rate of DNA by simple technology.
4 cl, 10 tbl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF OXIDE COMPOSITE COAT ON ALUMINIUM AND ITS ALLOYS | 2000 |
|
RU2169800C1 |
METHOD OF PRODUCING ZINC-NANODIAMOND ELECTROCHEMICAL COATING | 2016 |
|
RU2689355C1 |
METHOD OF PRODUCING ELECTROCHEMICAL SILVER COATING | 2015 |
|
RU2599471C1 |
METHOD OF ELECTROCHEMICAL SILVER-NANO-CARBON-DIAMOND COATING PRODUCING | 2015 |
|
RU2599473C1 |
METHOD OF OBTAINING ELECTROCHEMICAL COMPOSITE NICKEL-DIAMOND COATING | 2017 |
|
RU2676544C1 |
METHOD FOR SEALING OF ANODE OXIDE COATINGS ON ALUMINIUM AND ITS ALLOYS | 1993 |
|
RU2073752C1 |
METHOD OF PRODUCING OF BLACK WEAR-RESISTANT ANTI-CORROSION COATING ON ALUMINIUM AND ALUMINIUM BASED ALLOYS BY METHOD OF MICROARC OXYDATION | 2014 |
|
RU2570869C1 |
METHOD FOR MICRO-ARC OXIDATION | 2008 |
|
RU2389830C2 |
METHOD OF PRODUCING A POROUS COMPOSITE COATING | 2019 |
|
RU2713763C1 |
METHOD OF MAKING COATINGS | 2004 |
|
RU2252277C1 |
Authors
Dates
2017-09-21—Published
2016-02-11—Filed