FIELD: heat-exchanges processes. SUBSTANCE: heat carrier contains ethylene glycol, water, sodium tetraborate and, additionally, 4:1 mixture of high-boiling fraction with morpholine or 4:1 diethylamine-morpholine mixture, said high- boiling fraction being mixture of by-products from the stage of rectified morpholine isolation from catalysate in the process of production of morpholine from diethylene glycol and ammonia. EFFECT: increased heat resistance in the temperature range from minus 28-72 C to plus 205-245 C and reduced corrosive effect to carbon steel structural materials, and prevented foam formation. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
LIQUID HEAT CARRIER | 1998 |
|
RU2139907C1 |
COOLANT LIQUID FOR INTERNAL COMBUSTION ENGINE | 1996 |
|
RU2102428C1 |
CRUDE OIL DEHYDRATION AND DESALTING COMPOSITION | 1997 |
|
RU2139316C1 |
MIXTURE FOR DEHYDRATION AND SALT ELIMINATION OF PETROLEUM | 1997 |
|
RU2117689C1 |
COOLANT FLUID | 2003 |
|
RU2253663C1 |
DEMULSIFIER FOR DEHYDRATION AND DESALTING OF CRUDE OIL | 1995 |
|
RU2076134C1 |
HEAT CARRIER FOR SOLAR COLLECTOR | 2013 |
|
RU2557611C2 |
COMPOSITION FOR DEHYDRATION AND DESALTING OF CRUDE OIL | 1995 |
|
RU2076135C1 |
ABSORBING SOLUTION FOR ABSORPTION REFRIGERATING MACHINES | 0 |
|
SU1738818A1 |
METHOD OF PREPARING COOLING LIQUID | 1995 |
|
RU2103309C1 |
Authors
Dates
1999-10-20—Published
1998-02-24—Filed