FIELD: methods of dewatering of magnesium chloride solutions. SUBSTANCE: dewatering is carried out by spraying of solutions in boiling layer through pneumatic jets at gas velocity in layer of 1.5-3.5 m/s. Then, dewatered product is treated with neutral or acidified initial solution of magnesium chloride taken in amount ensuring content of magnesium chloride in desired product of not less than 50%. Subjected to treatment with initial solution of magnesium chloride may be dewatered product, cyclone dust, coarse or fine fraction of desired product. In this case, solution used for, treatment may by acidified with sulfuric or hydrochloric acid. EFFECT: improved service properties of magnesium chloride. 3 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DEHYDRATION OF SYNTHETIC CARNALLITE | 1999 |
|
RU2169702C2 |
METHOD OF DEHYDRATION OF SYNTHETIC CARNALLITE | 1998 |
|
RU2149141C1 |
METHOD OF DEHYDRATING MAGNESIUM CHLORIDE SOLUTIONS | 1997 |
|
RU2117630C1 |
METHOD OF DEHYDRATING SOLUTIONS OF CALCIUM OR MAGNESIUM CHLORIDE | 2003 |
|
RU2259947C2 |
METHOD OF PRODUCTION OF MAGNESIUM OXIDE | 2000 |
|
RU2186730C2 |
METHOD OF DEHYDRATING SYNTHETIC CARNALLITE | 1997 |
|
RU2123475C1 |
METHOD FOR PREPARING ANTI-GLAZE PREPARATION | 2002 |
|
RU2212428C1 |
METHOD FOR PRODUCTION OF MAGNESIUM FROM OXIDE-CHLORIDE RAW MATERIAL | 2001 |
|
RU2186155C1 |
METHOD OF PRODUCTION OF GRANULATED POTASSIUM CHLORIDE | 1999 |
|
RU2157356C1 |
METHOD OF TREATING OXIDE MAGNESIUM-CONTAINING RAW MATERIAL BEFORE ELECTROLYSIS | 2001 |
|
RU2200705C1 |
Authors
Dates
1999-11-10—Published
1998-05-20—Filed