FIELD: chemical industry. SUBSTANCE: amorphous silicon- containing material is subjected to mechanical and chemical treatment in 10-17 wt.% caustic soda solution at S:L ratio of 1:(2.5-3.5) at 25-50 C and atmospheric pressure for 4-8 h in ball mill. Method makes it possible to utilize effectively multi-ton dust waste resulting from amorphous microsilica (ferrosilicon) and to produce silicate adhesive bond used for making acid- resistant coatings, putties and mastics in chemical industry; heat-resistant (dense and porous) materials in metallurgy and heat and power engineering; gluing concrete products, brick, natural stone and finishing materials of different varieties in building industry. EFFECT: more efficient preparation method. 2 cl, 2 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF WATER GLASS | 2001 |
|
RU2187457C1 |
METHOD OF PREPARING ADHESIVE COMPOSITION | 1998 |
|
RU2152416C1 |
METHOD OF PRODUCING ALUMINOSILICATE GLUE BINDER | 2018 |
|
RU2674801C1 |
method of preparing thermoelectric material | 1996 |
|
RU2118669C1 |
METHOD OF PREPARING THE SOLID QUICK-SOLUBLE DISPERSED SYSTEM CONTAINING ACETYLSALICYLIC ACID | 1992 |
|
RU2099058C1 |
METHOD FOR PREPARATION OF MIXTURE FOR HARD ALLOYS BASED ON TUNGSTEN CARBIDE | 1996 |
|
RU2120840C1 |
METHOD OF MODIFYING CAST IRONS AND STEELS | 1996 |
|
RU2121510C1 |
METHOD OF PREPARING HEAT-RESISTANT INORGANIC PIGMENTS | 1997 |
|
RU2114886C1 |
METHOD OF ALKALINE-EARTH METAL ALUMINOSILICATE PRODUCING | 1993 |
|
RU2078037C1 |
METHOD OF PACKING SILICA DUST | 1998 |
|
RU2139245C1 |
Authors
Dates
2000-01-20—Published
1998-04-08—Filed