FIELD: chips processing, particularly, methods of chips briquetting. SUBSTANCE: chips are loosened and crushed to obtain members of two fractions 15-25 and 50-60 mm long. Produced fractions are mixed in weight ratio of 1: 5, washed in aqueous solution of labomide, dried at temperature of 180-220 C and compacted in press mold. EFFECT: stable high quality briquettes, namely, with low crumbling and high degree of purity. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING PRODUCTS OF CHIP | 2000 |
|
RU2161547C1 |
METHOD TO PELLETIZE METAL CHIP | 0 |
|
SU1734948A1 |
METHOD FOR BRIQUETTING OF METAL CHIPS | 2004 |
|
RU2267543C2 |
BRIQUETTING METHOD OF STEEL CUTTINGS | 2007 |
|
RU2354723C1 |
BRIQUETTE FOR METALLURGICAL TREATMENT | 2013 |
|
RU2549029C1 |
METAL CHIP BRIQUETTING METHOD | 2011 |
|
RU2490340C1 |
METHOD OF MANUFACTURE OF HEAT-INSULATING MEMBER | 1996 |
|
RU2135884C1 |
METHOD FOR BRIQUETTING METALLIC CHIP | 2003 |
|
RU2251580C2 |
BRIQUETTE FOR METALLURGICAL PRODUCTION | 2019 |
|
RU2710622C1 |
METHOD OF BRIQUETTING METAL CHIPS AND DEVICE FOR REALIZATION OF THIS METHOD | 2003 |
|
RU2266969C2 |
Authors
Dates
2000-03-20—Published
1998-07-14—Filed