FIELD: nonferrous metallurgy. SUBSTANCE: nitrogenization is carried out at 1200 C for 15 hr under pure nitrogen atmosphere followed by cooling, and annealing conducted for 1.5-2.5 hr under argon at 1200 C. EFFECT: increased heat resistance of parts made from alloys. 1 tbl, 8 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR HIGH-TEMPERATURE NITRIDING OF PARTS FROM STAINLESS AUSTENITIC STEELS | 2023 |
|
RU2824791C1 |
METHOD OF THE HIGH-TEMPERATURE NITRATION OF THE DETAILS MADE OUT OF THE CORROSION-RESISTANT NICKEL-CHROMIUM STEELS | 2004 |
|
RU2287608C2 |
METHOD FOR HIGH-TEMPERATURE NITROGENIZATION OF STEEL PARTS | 1998 |
|
RU2148676C1 |
METHOD FOR GAS NITRIDING PRODUCTS OF TITANIUM AND ITS ALLOYS | 0 |
|
SU1006540A1 |
METHOD FOR HIGH-TEMPERATURE NITROGENIZATION OF STEEL PARTS | 1998 |
|
RU2148677C1 |
METHOD FOR ANNEALING NITRIDED HIGH-MELTING METALS | 0 |
|
SU1041582A1 |
INTERNAL NITRATION OF FERRITE CORROSION-RESISTANT STEEL | 2012 |
|
RU2522922C2 |
METHOD FOR HARDENING PRODUCTS | 0 |
|
SU1027239A1 |
METHOD FOR ION NITRIDING OF PRODUCTS MADE OF CONSTRUCTION ALLOY STEELS | 2020 |
|
RU2760309C1 |
METHOD OF HARDENING TITANIUM ALLOYS IN GAS ENVIRONMENT | 2007 |
|
RU2365671C1 |
Authors
Dates
2000-05-10—Published
1998-06-26—Filed