FIELD: manufacture of polymeric binders for thermoplastic composite materials. SUBSTANCE: polyether is prepared by polycondensation of betulin with dicarboxylic acid such as pimelinic or azelainic or sebacinic acids at betulin to acid molar ratio of 1:(1.01-1.04). Process is carried out in inert medium under constant stirring at 256-260 C. EFFECT: increased degree of conversion of monomers in the process of preparing polyether and lower melting temperature thereof. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR POLYESTER PRODUCTION | 2004 |
|
RU2262516C1 |
METHOD FOR PRODUCING COPOLYMER BASED ON BETULIN | 2022 |
|
RU2798621C1 |
METHOD OF SYNTHESIS OF 1,2,4-TRIAZOLONE-5 | 1992 |
|
RU2085556C1 |
METHOD OF PREPARING 3-ACETYL-5,5-DIMETHYLHYDANTION | 1998 |
|
RU2131873C1 |
ELECTRIC INSULATING MATERIAL | 2003 |
|
RU2246146C1 |
METHOD OF SORPTION EXTRACTION OF CESIUM FROM NATURAL AND TECHNOLOGICAL WATERS | 1993 |
|
RU2065629C1 |
METHOD OF MANUFACTURING ION-EXCHANGE FIBER | 2000 |
|
RU2194809C2 |
METHOD OF MANUFACTURING TEXTILE CATALYST ON FIBERGLASS CARRIER | 1998 |
|
RU2134613C1 |
TEXTILE FIBROUS BULKED CATALYST | 1997 |
|
RU2118908C1 |
METHOD OF REMOVING SULFIDES FROM WASTE WATERS | 1995 |
|
RU2099292C1 |
Authors
Dates
2001-05-27—Published
1999-10-06—Filed