FIELD: applying coatings by gas thermal methods. SUBSTANCE: method comprises electric-spark alloying in argon provided that following conditions are observed: specific time of alloying is 1.5-2 min/sq.cm, discharge current is 0.4-0.6A, electrode vibration amplitude is 100 Hz. EFFECT: greater strength of adhesion of coating with surface of products. 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARATION OF THE SURFACE BEFORE DEPOSITION OF THE PLASMA COATINGS | 2005 |
|
RU2294394C2 |
SYRINGE | 1999 |
|
RU2169583C1 |
METHOD OF RUNNING-IN KINEMATIC FRICTION PAIRS | 1998 |
|
RU2152543C1 |
BEE FEED PREPARING LINE | 2001 |
|
RU2192127C1 |
APPARATUS FOR EXTRACTING MILK FROM COW UDDER SHARES DISEASED WITH MASTITIS | 2000 |
|
RU2189133C2 |
METHOD OF DEPOSITING OF A CHROMIUM COATING ON STEEL DETAILS | 2004 |
|
RU2269608C1 |
METHOD FOR EXTRACTING OF BEE-BREAD FROM COMBS | 2005 |
|
RU2297763C1 |
METHOD FOR RESTORING GEAR TRANSMISSIONS | 2001 |
|
RU2213650C2 |
UNIT FOR MILKING OUT AND CONTROLLING OF FIRST MILK STREAMS | 2000 |
|
RU2185054C2 |
APPARATUS FOR DISINFECTING UDDER TEATS AFTER MILKING | 2000 |
|
RU2212788C2 |
Authors
Dates
2001-09-10—Published
1999-10-12—Filed