FIELD: preparation of aluminium hydroxide and alumina. SUBSTANCE: method comprises decomposing aluminate solution in the presence of seed, filtering aluminium hydroxide and drying thereof. During drying process, aluminium hydroxide is classified to grain size of less than 40 mcm. Dry aluminium hydroxide having fraction of less than 40 mcm is used as seed for decomposing aluminate solution or as commercial product. Dry aluminium hydroxide having fraction of greater than 40 mcm is calcined to give larger aluminium oxide. EFFECT: reduced content of impurities in the resulting product. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING LOW-ALKALI ALUMINA | 1992 |
|
RU2047561C1 |
ALUMINATE SOLUTION DECOMPOSITION METHOD | 2002 |
|
RU2231497C1 |
METHOD OF PROCESSING LOW-GRADE BAUXITE INTO SILICA ACCORDING TO SUCCESSIVE BEYER-SINTERING SCHEME | 1996 |
|
RU2113406C1 |
METHOD FOR PROCESSING NEPHELINE | 1991 |
|
RU2015107C1 |
METHOD OF PROCESSING OF BAUXITES INTO ALUMINA | 1999 |
|
RU2181695C2 |
METHOD OF PROCESSING ALUMINATE SOLUTION IN PRODUCTION OF ALUMINA FROM NEPHELINE | 2000 |
|
RU2184703C2 |
METHOD OF ALUMINATE SOLUTION DECOMPOSITION OPERATION | 1991 |
|
RU2051099C1 |
METHOD FOR PRODUCTION OF ALUMINIUM HYDROXIDE | 1992 |
|
RU2038303C1 |
PLANT FOR PRODUCTION OF ALUMINA FROM RAW ALUMINIUM HYDROXIDE | 1996 |
|
RU2093465C1 |
METHOD OF PROCESSING ALUMINATE SOLUTIONS | 2000 |
|
RU2200706C2 |
Authors
Dates
2001-11-10—Published
1997-07-08—Filed