FIELD: mechanical engineering. SUBSTANCE: method involves manufacturing investment pattern from powdered mixture of single- component investment pattern material of 0.1-1.6 mm fraction and boric acid of 0.01-0.3 mm fraction, with volumetric ratio of components being, %: investment pattern material 75-80, boric acid 20-25; providing dosed dispensing of investment pattern material into mold in an amount providing manufacture of investment patterns with porosity of 3- 10%; pressing investment pattern material without preliminary heating by aligning detachment surfaces of mold. During pressing powdered investment pattern material is caked without substantial development of deformation processes and with formation of open capillary porosity providing compensation of investment pattern in the process of heating during melting from ceramic enclosure. Method is used for investment casting. EFFECT: increased efficiency by improved dimensional and geometric precision of investment patterns and ingots. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF REMOVABLE INVESTMENT PATTERNS | 2001 |
|
RU2185922C1 |
METHOD FOR MANUFACTURE OF REMOVABLE INVESTMENT PATTERNS | 2001 |
|
RU2185920C1 |
METHOD FOR MANUFACTURE OF REMOVABLE INVESTMENT PATTERNS | 2000 |
|
RU2185919C2 |
METHOD FOR MAKING INVESTMENT PATTERNS | 2000 |
|
RU2188737C2 |
METHOD FOR MANUFACTURE OF REMOVABLE PATTERNS | 2000 |
|
RU2193469C2 |
METHOD FOR MAKING INVESTMENT PATTERNS | 2000 |
|
RU2188736C2 |
METHOD FOR MAKING INVESTMENT PATTERNS | 2000 |
|
RU2188734C2 |
METHOD OF MANUFACTURE OF DISPOSABLE PATTERNS | 2000 |
|
RU2189885C2 |
METHOD FOR MANUFACTURE OF REMOVABLE INVESTMENT PATTERNS | 2001 |
|
RU2185923C1 |
METHOD FOR MANUFACTURE OF REMOVABLE INVESTMENT PATTERNS | 2001 |
|
RU2185924C1 |
Authors
Dates
2002-07-27—Published
2001-02-26—Filed