FIELD: inorganic compounds technology. SUBSTANCE: lithium hydroxide and niobium oxide are ground to particle size less than 1 mcm. Mixture is dehydrated and heated in oxygen-containing gas flow (70-100 vol.% oxygen and 0.01-0.05 wt. % moisture) to 850- 900 C at heating rate 1-20 C/min, preferably 4-10 C/min. Product is suited to application in electronic engineering. EFFECT: reduced power consumption and increased yield of single-phase powdered product. 5 cl, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF PREPARING LITHIUM METHATANTALATE | 2001 | 
 | RU2188160C1 | 
| METHOD OF PRODUCTION OF ALKALINE METAMETALS (V) AND SOLID SOLUTIONS ON THEIR BASE | 2004 | 
 | RU2259948C1 | 
| METHOD OF DECOMPOSITION OF WASTES OF REFRACTORY METALS WITH LITHIUM COMPOUND MONOCRYSTALS PRODUCTION | 2002 | 
 | RU2221746C2 | 
| PROCESS FOR PRODUCING ALKALI AND/OR ALKALI EARTH METAL NIOBATES, TANTALATES AND VANADATES | 0 | 
 | SU994414A1 | 
| CATALYST FOR OXIDATION OF O-OXYLENE OR NAPHTHALENE TO PHTHALTIC ANHYDRIDE | 0 | 
 | SU1147244A3 | 
| PROCESS FOR PRODUCING TANTALUM PENTOXIDE | 0 | 
 | SU973482A1 | 
| METHOD OF DISSOLVING AND PURIFYING TANTALUM PENTAOXIDE (VARIANTS) | 1996 | 
 | RU2171229C2 | 
| METHOD OF PRODUCTION OF CUPROUS-ALUMINUM SPINEL EXTRUDATES | 1999 | 
 | RU2225253C2 | 
| METHOD FOR PREPARATION OF NANODIMENSIONAL FERROELECTRIC POWDER | 2007 | 
 | RU2362741C1 | 
| NIOBIUM SUBOXIDE, METHOD OF ITS PREPARATION AND CAPACITOR CONTAINING NIOBIUM SUBOXIDE AS ANODE | 2004 | 
 | RU2363660C2 | 
Authors
Dates
2002-08-27—Published
2001-06-14—Filed