FIELD: rubber industry. SUBSTANCE: polydimethylsiloxane rubber is modified by UV irradiation in presence of photoinitiator and reagent forming active groups, said photoinitiator being organic carbonyl-containing compounds selected from aromatic ketone and quinone series, taken in amounts 0.001-0.01 mole/1 kg rubber, at 50-150 C for 30-90 min in atmosphere of air oxygen as above- mentioned reagent. Thus formed active groups are further substituted by reaction with oxygen- or nitrogen-containing substituting reagents such as amines, amino acids, hydrazines, alcohols, and orthoethers. EFFECT: enabled production of rubber with specified structure. 1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HARDENING HIGH-MOLECULAR POLYDIMETHYLSILOXANE RUBBER | 2001 |
|
RU2196149C2 |
COMPOSITE MATERIAL PREPARATION METHOD | 2002 |
|
RU2229485C1 |
METHOD OF SILOXANE RUBBER HARDENING | 0 |
|
SU1694599A1 |
METHOD OF MODIFYING POLYDIMETHYLSILOXANE | 2013 |
|
RU2550364C1 |
FLUORINE RUBBER-BASED COATING FORMATION METHOD | 2002 |
|
RU2232780C2 |
POLYMER PHOTOINITIATORS | 2011 |
|
RU2572839C2 |
DEGRADABLE PHOTO CROSS-LINKING AGENT | 2011 |
|
RU2594729C2 |
METHOD OF PROCESSING RUBBER-CURE WASTES OF HIGH-MOLECULAR SILOXANE RUBBERS | 1995 |
|
RU2086577C1 |
COMPOSITION AND METHOD FOR ITS HARDENING | 1997 |
|
RU2210798C2 |
METHOD OF MANUFACTURING ELECTROCHROMIC DEVICE AND ELECTROCHROMIC DEVICE | 2016 |
|
RU2642558C1 |
Authors
Dates
2003-01-20—Published
2001-03-30—Filed