FIELD: metallurgy. SUBSTANCE: method involves charging and melting in furnace burden comprising titanium oxides, reducer, and iron thermit settler. Ferroaluminum used as a reducer contains 55-60% of aluminum. Method allows alloy with titanium content of 50-60% to be produced. EFFECT: increased efficiency and provision for obtaining ferrotitanium of homogeneous chemical and phase composition. 7 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING BURDEN FROM IRON BASED POWDERS | 2000 |
|
RU2190669C2 |
METHOD OF MANUFACTURE OF CONSUMABLE ELECTRODE | 1994 |
|
RU2083326C1 |
METHOD FOR ELECTROSLAG FERROTITANIUM SMELTING | 1993 |
|
RU2039101C1 |
METHOD OF PRODUCING CASTINGS FROM NONCOMPACT STEEL WASTES AND DEVICE FOR PRESSING BLOCKS OF STEEL CONSUMABLE ELECTRODES FOR METHOD EMBODIMENT | 1999 |
|
RU2148665C1 |
CHARGE FOR PRODUCTION OF NITROGEN-CONTAINING MASTER ALLOYS ON BASE OF REFRACTORY METALS | 2001 |
|
RU2206628C2 |
METHOD OF ALUMINO-THERMAL PRODUCTION OF FERRO-TITANIUM | 2006 |
|
RU2338805C2 |
STOCK FOR FERROTITANIUM PRODUCTION | 2006 |
|
RU2325456C2 |
METHOD OF WORKING SEMIFINISHED PRODUCT SURFACES | 2000 |
|
RU2174461C1 |
METHOD FOR PRODUCING OF FERROTITANIUM ALLOYS | 2006 |
|
RU2308501C1 |
METHOD FOR PRODUCING OF INGOTS | 2003 |
|
RU2263721C2 |
Authors
Dates
2003-01-20—Published
2000-11-30—Filed