FIELD: industrial explosives, applicable for crushing of rock. SUBSTANCE: the method consists in grinding of powder composition to obtain powder crumb, mixing of powder crumb with ammonium nitrate and pressing of the charge, grinding of powder composition is accomplished at water irrigation, after grinding water pressing of powder crumb is conducted and final removal of water by suction of hot air through the formed charge. EFFECT: enhanced safety of manufacture of industrial explosives based on pyroxilin powder and ammonium nitrate, possessing mechanical strength and definite geometric dimensions. 2 cl, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
EXPLOSIVE | 2007 |
|
RU2382755C2 |
INDUSTRIAL EXPLOSIVE SUBSTANCE | 2012 |
|
RU2525550C2 |
GUNPOWDER EXPLOSIVE COMPOSITION AND A METHOD FOR PREPARATION THEREOF | 2002 |
|
RU2226522C2 |
"POROTOL" INDUSTRIAL EXPLOSIVE COMPOUND | 1996 |
|
RU2126780C1 |
METHOD FOR RECOVERY OF SOLID-PROPELLANT CHARGE (ALTERNATIVES) | 1999 |
|
RU2176230C2 |
METHOD OF RECYCLING EXPLOSIVE MATERIALS AND APPARATUS FOR REALISING SAID METHOD | 2011 |
|
RU2485078C2 |
EXPLOSIVE | 1995 |
|
RU2103248C1 |
EXPLOSIVE COMPOSITION | 2000 |
|
RU2180328C1 |
POWDER EXPLOSIVE COMPOSITION | 1998 |
|
RU2122990C1 |
METHOD OF BALLISTIC SOLID ROCKET PROPELLANTS | 2012 |
|
RU2499980C1 |
Authors
Dates
2003-04-27—Published
2001-05-15—Filed