FIELD: mineral fibers. SUBSTANCE: invention concerns mineral wool capable of being dissolved in physiologic medium and including following components, wt %: SiO2 38-52, Al2O2 16-23, RO(Ca+MgO) 4-15, R2O(Na2O+K2O) 16-25, B2O3 0-10, Fe2O3 (total amount of iron) 0-3, preferably 0-1.5, P2O5 0-3, preferably 0-1.5, TiO2 0-2. Dissolution rate of wool in physiologic medium is at least 30 ng/sq.m.hr. Mineral wool is manufactured by means of internal centrifugation. EFFECT: optimized wool composition and improved its capacity for biological degradation. 15 cl, 2 tbl