FIELD: explosives. SUBSTANCE: invention provides method for manufacturing spherical gunpowder comprising (i) 10-15-min stirring, in an aqueous medium, of mixture of pyroxyline with recycled process wastes or stirring of recycled process wastes with aqueous suspension of carbon black; (ii) preparing gun powder lacquer in ethyl acetate for 60 to 180 min; (iii) dispersing lacquer onto spherical particles; and (iv) removing ethyl acetate on heating of mixture to 92-94 C, said recycled process wastes being pyroxyline or ballistic powder in amounts between 10 and 100 wt %. EFFECT: enabled reuse of powders with expired storage term. 3 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF PELLET POWDER | 2003 |
|
RU2256636C1 |
METHOD OF PRODUCING SPHERICAL POWDER FOR 5,6 MM-SPORTING CALIBER CARTRIDGES WITH ANNULAR IGNITION | 2010 |
|
RU2451652C2 |
POROUS SPHERICAL GUNPOWDER MANUFACTURE METHOD | 2003 |
|
RU2258688C2 |
METHOD FOR PRODUCTION OF SPHERICAL POWDER FOR SPORT HUNTING CARTRIDGE 30 CARBINE (7,62×33) | 2010 |
|
RU2452720C2 |
METHOD OF PRODUCTION OF THE SPHERICAL POWDER | 2004 |
|
RU2280634C1 |
EMULSION METHOD FOR PROCESSING GUNPOWDERS | 2001 |
|
RU2201912C2 |
METHOD OF PRODUCING PYROXYLINE PELLET POWDER FOR 7,62 MM SPORT CARTRIDGE | 2015 |
|
RU2597391C2 |
METHOD OF PRODUCTION OF SPHERICAL POWDER FOR SHOT CARTRIDGES FOR SMOOTH-BORE SPORTS AND HUNTING WEAPONS OF 12, 16 AND 20 CALIBRE | 2012 |
|
RU2522642C2 |
METHOD FOR PRODUCTION OF SPHERICAL POWDER FOR 5,6 MM SPORT HUNTING CARTRIDGE OF CIRCULAR IGNITION | 2010 |
|
RU2452721C2 |
METHOD OF MAKING POROUS SPHERICAL POWDER FOR SMOOTH-BORE GUN SHOT CARTRIDGES | 2010 |
|
RU2451656C2 |
Authors
Dates
2004-03-27—Published
2002-04-05—Filed