FIELD: production of pellet powders for small-arms, for example for smooth-bore shot-firing guns.
SUBSTANCE: proposed method includes preparation of powder lacquer at mixing nitrocellulose ingredients in 4-5 mass parts of water with ethyl acetate, adding emulsifying agent, dispersing lacquer and removing solvent. Used as nitrocellulose ingredients are pyroxiline with ballistic powder or fine-grained pyroxiline powder with ballistic powder or all together: pyroxyline, fine-grained pyroxyline powder and ballistic powder at content of one of nitrocellulose ingredients not exceeding 30 mass-%. Emulsifying agent is added in the amount not exceeding 20-30 mass-% of total amount; dispersion of lacquer is continued for 10-20 min; then, process is discontinued for 10-20 min, after which dispersion is repeated and is continued for 10-20 min at introduction of remaining amount of emulsifying agent; hide glue is used as emulsifying agent. At content of one of nitrocellulose ingredients not exceeding 10 mass-%, dispersion cycle is repeated twice.
EFFECT: enhanced stability of ballistic characteristics of powder due to smooth distribution of components in volume.
2 cl, 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING SPHERICAL GUNPOWDER | 2002 |
|
RU2226184C2 |
METHOD FOR DISTILLATION OF DISSOLVENT FROM POWDER ELEMENTS OF PELLET POWDER | 2010 |
|
RU2452718C2 |
METHOD OF PELLET POWDERS PRODUCING | 2015 |
|
RU2605252C2 |
POROUS SPHERICAL GUNPOWDER MANUFACTURE METHOD | 2003 |
|
RU2258688C2 |
METHOD OF PRODUCING COARSELY DISPERSED PELLET POWDER | 2009 |
|
RU2439042C2 |
METHOD OF PREPARING PELLET POWDER | 2008 |
|
RU2422417C2 |
EMULSION METHOD FOR PROCESSING GUNPOWDERS | 2001 |
|
RU2201912C2 |
METHOD OF PREPARING PELLET POWDER | 2007 |
|
RU2386607C2 |
METHOD OF MAKING POROUS SPHERICAL POWDER FOR SMOOTH-BORE GUN SHOT CARTRIDGES | 2010 |
|
RU2451656C2 |
METHOD OF PRODUCING BALL POWDER | 2015 |
|
RU2622129C1 |
Authors
Dates
2005-07-20—Published
2003-11-26—Filed