FIELD: production of metallic powders by spraying. SUBSTANCE: method comprising steps of heating melt metal in steel melting aggregate, draining it to steel casting ladle, spraying by compressed air. In order to produce raw powder according to invention method comprises steps of preparing metallic raw powder with predetermined fraction size by spraying melt through slide valve rigidly secured to steel casting ladle and having calibration opening with diameter 11-13 mm at temperature of melt in spraying zone 1400-1450C. EFFECT: enhanced efficiency due to increased yield of high quality powder. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PLASMA-LIQUID PRODUCTION OF METAL POWDERS FROM 3D PRINTING PRODUCTS | 2022 |
|
RU2802608C1 |
METHOD OF PRODUCING STAINLESS STEEL POWDER AND APPARATUS FOR PRODUCING SAID POWDER | 2023 |
|
RU2823268C1 |
METHOD OF PRODUCTION OF THE CARBON STEEL | 2006 |
|
RU2304622C1 |
METHOD OF STEEL SMELTING, DEOXIDATION, ALLOYING AND TREATMENT | 2009 |
|
RU2405046C1 |
METHOD FOR DIRECT PRODUCTION OF METALS FROM MATERIALS CONTAINING IRON OXIDES (VERSIONS) AND DEVICE FOR IMPLEMENTING IT | 2012 |
|
RU2548871C2 |
DEVICE FOR DOZED RELEASE OF METAL FROM TANK | 1993 |
|
RU2042472C1 |
COMBINATION VACUUM INDUCTION ELECTRON BEAM FURNACE FOR MELTING, REFINING AND CASTINY OF METAL | 1992 |
|
RU2093768C1 |
METHOD OF IRON POWDER RECEIVING | 2007 |
|
RU2360769C2 |
VANADIUM SLAG TREATMENT METHOD | 1997 |
|
RU2105073C1 |
PREPARATION OF METALLURGICAL LADLE | 2013 |
|
RU2569198C2 |
Authors
Dates
2004-05-27—Published
2002-05-31—Filed