FIELD: processes for making gun barrels, possibly for all types of firearms. SUBSTANCE: blank of gun barrel includes steel rod made at least of two types of steel. At least one of said two types of steel is in the form of powder steel. Rod is subjected to multiple twisting around its lengthwise axis during one or several stapes of how working. Rod is twisted until leading angle of helical line in range 45 - 90 degrees. Then twisted rod is drilled or punched along its lengthwise axis. EFFECT: enhanced strength properties of gun barrel. 10 cl, 3 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING CERAMIC INSERT FOR GUN BARRELS | 2016 |
|
RU2647948C2 |
METHOD OF PRODUCTION OF GUN BARREL | 2013 |
|
RU2557892C2 |
GUN BARREL | 2013 |
|
RU2602163C2 |
METHOD OF CLEANING OF GUN BARRELS AND COMPOSITION OF CLEANING AGENTS | 1995 |
|
RU2128319C1 |
METHOD OF MANUFACTURING COMPOSITE METAL ARTICLE | 1995 |
|
RU2127195C1 |
WORKPIECE FOR PRODUCT WITH DAMASCENE PATTERN | 2019 |
|
RU2790131C2 |
METHOD OF MANUFACTURE OF THE MULTILAYERED STAINLESS METAL PRODUCTS | 2005 |
|
RU2288101C1 |
METHOD OF PRODUCING COMPOSITE METAL PLATE WITH PATTERN | 2017 |
|
RU2737527C1 |
ALL-PURPOSE GUN LUBRICANT | 2020 |
|
RU2723631C1 |
ACCESSORY FOR FIREARM | 2014 |
|
RU2672756C2 |
Authors
Dates
2004-06-10—Published
2000-02-02—Filed