FIELD: electrical engineering.
SUBSTANCE: paste contains 72-89% lead oxides, 10-22% lead sulfates, 0.48-8.0% lead metal, and 0.001-1.0% fulleroid-type nano-modifier, in particular fullerens C60 and C70 or their mixtures, nanotubes and polyhedral layered carbon fulleroid-type nanostructures. Preparation of paste consists in mixing lead powder with 0.001 to 1.0% of indicated modifier.
EFFECT: increased service time of lead accumulator and simplified preparation of paste with coarse-grained structure.
5 cl, 5 dwg, 1 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
PASTE FOR POSITIVE ELECTRODE OF LEAD BATTERY | 2010 |
|
RU2443039C1 |
PROCESS OF MANUFACTURE OF POSITIVE ELECTRODE OF LEAD-ACID CELL | 1991 |
|
RU2025002C1 |
LAYERED FULLEROID-TYPE POLYHEDRAL CARBON NANOSTRUCTURES | 2000 |
|
RU2196731C2 |
BATTERY PASTE AND METHOD FOR ITS PREPARATION | 2014 |
|
RU2611879C2 |
PASTE FOR POSITIVE ELECTRODE OF LEAD ACCUMULATOR | 2010 |
|
RU2446513C1 |
COMPOSITION FOR MANUFACTURE OF BUILDING MATERIALS | 2000 |
|
RU2233254C2 |
SINTERED COMPOSITE MATERIAL | 2016 |
|
RU2635059C2 |
PASTE FOR NEGATIVE ELECTRODE OF LEAD-ACID BATTERY AND METHOD OF ITS PREPARATION | 2011 |
|
RU2454756C1 |
ANTIFRICTION COMPOSITION MATERIAL | 2002 |
|
RU2237685C2 |
NONLINEAR OPTICAL ELEMENT FOR LIMITING ELECTROMAGNETIC RADIATION FLOWS | 2001 |
|
RU2238577C2 |
Authors
Dates
2004-09-27—Published
2002-06-10—Filed