FIELD: chemical industry.
SUBSTANCE: the invention is intended for chemical industry. To 1 g of a powder of nanodiamonds of an explosive synthesis add 100 ml deionized water. The mixture is treated with the ultrasonic dispersant for 5 minutes. The produced suspension is added with an electrolyte - NaCl solution in the quantity exceeding sorptive capacity of nanoparticles by ions of sodium, for example, 20 ml of 0.9 M solution. Then separate the disperse medium and the settling. The disperse medium is removed. The settling is added with 100 ml of deionized water and is intensively agitated. The supernatant - hydrosol of nanodiamonds is separated and dried. At multiple add-on of water to the produced powder a stable nanodiamond hydrosol is formed. The share of the surface impurities in the produced nanodiamond is reduced. Simultaneously the share of sodium ions is increased.
EFFECT: the invention allows to reduce the share of the surface impurities in the produced nanodiamond and simultaneously to increase the share of sodium ions.
1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
NANO-SIZE DIAMOND TREATMENT METHOD | 2003 |
|
RU2258671C2 |
METHOD OF EXTRACTING HIGH COLLOIDAL STABILITY DETONATION SYNTHESIS NANODIAMONDS | 2010 |
|
RU2458858C1 |
OPTICAL RADIATION POWER INTENSITY LIMITING WORKING MEDIUM AND PREPARATION METHOD THEREOF | 2009 |
|
RU2410737C1 |
SYNTHETIC DIAMOND-CONTAINING SUBSTANCES AND A METHOD FOR SEPARATION THEREOF | 2006 |
|
RU2306258C1 |
NANODIAMOND SORBENT AND METHOD OF ITS OBTAINING | 2007 |
|
RU2352387C1 |
ISOLATION METHOD FOR NATURAL AND RECOMBINANT PROTEINS AND OTHER BIOLOGICAL COMPOUNDS | 2007 |
|
RU2366713C2 |
LUBRICATING COMPOSITION | 2007 |
|
RU2356938C2 |
METHOD OF NANODIAMONDS TREATMENT | 2008 |
|
RU2367596C1 |
METHOD OF RECEIVING OF NICKEL-ADAMANTINE CHEMICAL COATINGS | 2007 |
|
RU2357002C1 |
METHOD OF PRODUCTION OF METAL-DIAMOND CHEMICAL COATING | 2007 |
|
RU2375494C2 |
Authors
Dates
2005-05-20—Published
2003-06-26—Filed