FIELD: metallurgy.
SUBSTANCE: working walls of crystallizer are restored without dismounting them. At first condition of working surfaces of walls is detected. If lower portions of surfaces of narrow and wide walls near angles of crystallizer are worn and central portion of narrow walls are not worn, shot blasting of worn surface is performed. Then coating is applied onto said zone by gasothermic deposition. Residual wear degree is no less than 0.5 - 0.6 mm. If central portion of narrow walls is not worn it is provided improved strength of deposited coating.
EFFECT: enhanced strength of deposited coating.
2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RESTORATION OF WORKING SURFACES OF CRYSTALLIZER WALLS | 2005 |
|
RU2286228C1 |
METHOD FOR RECOVERY OF CRYSTALLIZER WORKING WALL | 2001 |
|
RU2186654C1 |
METHOD FOR RECONDITIONING MOLD WORKING WALLS | 1997 |
|
RU2119404C1 |
METHOD FOR RESTORING THE WORK SURFACE OF CRYSTALLISER WALLS | 2015 |
|
RU2624878C2 |
METHOD OF PREPARING STEEL POURING CRYSTALLIZER FOR OPERATION | 1996 |
|
RU2106225C1 |
PROCESS OF REPAIR OF MOULD FOR CONTINUOUS CASTING OF STEEL | 1997 |
|
RU2118228C1 |
METHOD FOR REPAIRING NARROW WALLS OF MOLD OF MACHINE FOR CONTINUOUS STEEL CASTING | 2000 |
|
RU2202440C2 |
METHOD OF RESTORATION OF WORKING WALLS OF CRYSTALLISER MADE OF COPPER OR ITS ALLOYS | 2006 |
|
RU2333087C2 |
METHOD FOR MANUFACTURE OF MOLD FOR STEEL CONTINUOUS CASTING | 1997 |
|
RU2113934C1 |
METHOD FOR PREPARING OF BLAST FURNACE TUYERE FOR OPERATION | 2005 |
|
RU2308491C2 |
Authors
Dates
2006-02-20—Published
2004-06-25—Filed